erosion
Leading-edge erosion estimated 32% of LEP (leading-edge-protection) coating loss over 20 m outer span. AEP loss correlation: 1.5-2.5% per DNV-RP-0573 erosion-impact curves.
Same canonical CoatingPassport data product as every other Hullproof vertical, applied to a wind turbine blade. Domain knowledge (applicable standards, severity calibration) is automatically applied via the domain registry — adding a new asset class is a directory, not a rewrite.
Leading-edge erosion estimated 32% of LEP (leading-edge-protection) coating loss over 20 m outer span. AEP loss correlation: 1.5-2.5% per DNV-RP-0573 erosion-impact curves.
Localized bond-line delamination, ~0.6 m² at shear web. Structural significance moderate per DNV-RP-0573.
Surface crack ~45 mm at trailing edge, tip section. Below 200 mm propagation threshold.
The same JSON powers Cognite CDF Asset+Timeseries, OSDU exports, RDF knowledge graphs, and MCP-tool calls from agentic systems. PDF is a renderer of this; never the source.