anode depletion
Anode array 82% depleted across A1-A4. Exceeds DNV-RP-B401 80% threshold for subsea structures where retrofit options are limited.
Annual GVI on an 8-slot production manifold (commissioned 2008, 326 m water depth) by work-class ROV. Findings emphasize the CP retrofit window — anode array 82% depleted, exceeding DNV-RP-B401 80% threshold for subsea structures where retrofit options are limited. Marine growth impedes weld-access; coating breakdown from prior intervention damage.
Anode array 82% depleted across A1-A4. Exceeds DNV-RP-B401 80% threshold for subsea structures where retrofit options are limited.
Marine growth 80-90 mm thickness on upper structural members. Impedes ROV access for close-visual inspection of critical welds.
Localized surface corrosion at hub-connector C-3 collar interface, estimated 6% wall-thickness loss. Within NORSOK U-009 monitoring threshold.
NORSOK M-501 coating system breakdown ~12% over a 3 m × 0.5 m frame-member section. Active corrosion at breakdown perimeter. Consistent with ROV-impact damage from prior intervention.